TYPICAL PROPERTIES (1) |
MECHANICAL |
Value |
Unit |
Standard |
Taber Abrasion, CS-17, 1 kg |
10 |
mg/1000cy |
SABIC Method |
Tensile Stress, yield, 50 mm/min |
63 |
MPa |
ISO 527 |
Tensile Stress, break, 50 mm/min |
60 |
MPa |
ISO 527 |
Tensile Strain, yield, 50 mm/min |
6 |
% |
ISO 527 |
Tensile Strain, break, 50 mm/min |
85 |
% |
ISO 527 |
Tensile Modulus, 1 mm/min |
2350 |
MPa |
ISO 527 |
Flexural Stress, yield, 2 mm/min |
90 |
MPa |
ISO 178 |
Flexural Modulus, 2 mm/min |
2300 |
MPa |
ISO 178 |
Hardness, H358/30 |
95 |
MPa |
ISO 2039-1 |
IMPACT |
Value |
Unit |
Standard |
Izod Impact, unnotched 80*10*3 +23°C |
NB |
kJ/m² |
ISO 180/1U |
Izod Impact, unnotched 80*10*3 -30°C |
NB |
kJ/m² |
ISO 180/1U |
Izod Impact, notched 80*10*3 +23°C |
70 |
kJ/m² |
ISO 180/1A |
Izod Impact, notched 80*10*3 -30°C |
12 |
kJ/m² |
ISO 180/1A |
Charpy 23°C, V-notch Edgew 80*10*3 sp=62mm |
73 |
kJ/m² |
ISO 179/1eA |
Charpy -30°C, V-notch Edgew 80*10*3 sp=62mm |
14 |
kJ/m² |
ISO 179/1eA |
Charpy 23°C, Unnotch Edgew 80*10*3 sp=62mm |
NB |
kJ/m² |
ISO 179/1eU |
Charpy -30°C, Unnotch Edgew 80*10*3 sp=62mm |
NB |
kJ/m² |
ISO 179/1eU |
Charpy Impact, notched, 23°C |
30 |
kJ/m² |
ISO 179/2C |
THERMAL |
Value |
Unit |
Standard |
Thermal Conductivity |
0.2 |
W/m-°C |
ISO 8302 |
CTE, 23°C to 80°C, flow |
7.E-05 |
1/°C |
ISO 11359-2 |
Ball Pressure Test, 125°C +/- 2°C |
PASSES |
- |
IEC 60695-10-2 |
Vicat Softening Temp, Rate B/50 |
141 |
°C |
ISO 306 |
Vicat Softening Temp, Rate B/120 |
142 |
°C |
ISO 306 |
HDT/Be, 0.45MPa Edgew 120*10*4 sp=100mm |
136 |
°C |
ISO 75/Be |
HDT/Ae, 1.8 MPa Edgew 120*10*4 sp=100mm |
125 |
°C |
ISO 75/Ae |
Relative Temp Index, Elec |
130 |
°C |
UL 746B |
Relative Temp Index, Mech w/impact |
120 |
°C |
UL 746B |
Relative Temp Index, Mech w/o impact |
125 |
°C |
UL 746B |
PHYSICAL |
Value |
Unit |
Standard |
Mold Shrinkage on Tensile Bar, flow (2) (5) |
0.5 - 0.7 |
% |
SABIC Method |
Density |
1.2 |
g/cm³ |
ISO 1183 |
Water Absorption, (23°C/sat) |
0.35 |
% |
ISO 62 |
Moisture Absorption (23°C / 50% RH) |
0.15 |
% |
ISO 62 |
Melt Volume Rate, MVR at 300°C/1.2 kg |
9 |
cm³/10 min |
ISO 1133 |
OPTICAL |
Value |
Unit |
Standard |
Haze, 2.54 mm |
NA |
% |
ASTM D 1003 |
Refractive Index |
NA |
- |
ISO 489 |
ELECTRICAL |
Value |
Unit |
Standard |
Volume Resistivity |
>1.E+15 |
Ohm-cm |
IEC 60093 |
Surface Resistivity, ROA |
>1.E+15 |
Ohm |
IEC 60093 |
Dielectric Strength, in oil, 3.2 mm |
17 |
kV/mm |
IEC 60243-1 |
Relative Permittivity, 1 MHz |
2.7 |
- |
IEC 60250 |
Dissipation Factor, 50/60 Hz |
0.001 |
- |
IEC 60250 |
Dissipation Factor, 1 MHz |
0.01 |
- |
IEC 60250 |
Comparative Tracking Index |
225 |
V |
IEC 60112 |
Relative Permittivity, 50/60 Hz |
2.7 |
- |
IEC 60250 |
FLAME CHARACTERISTICS |
Value |
Unit |
Standard |
UL Recognized, 94V-0 Flame Class Rating (3) |
1 |
mm |
UL 94 |
Glow Wire Flammability Index 850°C, passes at |
1 |
mm |
IEC 60695-2-12 |
Glow Wire Flammability Index 960°C, passes at |
1.6 |
mm |
IEC 60695-2-12 |
Oxygen Index (LOI) |
35 |
% |
ISO 4589 |