规格与认可

Mobilgear 600 XP 系列 符合或超越以下要求 Mobilgear 600 XP 68 Mobilgear 600 XP 100 Mobilgear 600 XP 150 Mobilgear 600 XP 220 Mobilgear 600 XP 320 Mobilgear 600 XP 460 Mobilgear 600 XP 680
AGMA 9005-E02 2 EP 3 EP 4 EP 5 EP 6 EP 7 EP -
DIN 51517-3: 2009-06 X X X X X X X
ISO 12925-1 Typ CKD 68 CKD 100 CKD 150 CKD 220 CKD 320 CKC 460 CKC 680
Mobilgear 600 XP 系列 获得以下制造商的认可 Mobilgear 600 XP 68 Mobilgear 600 XP 100 Mobilgear 600 XP 150 Mobilgear 600 XP 220 Mobilgear 600 XP 320 Mobilgear 600 XP 460 Mobilgear 600 XP 680
SIEMENS AG Flender gear units, T 7300, Table A-a, Flender Code No.   A17 A16 A15 A14 A13 A12
SIEMENS AG Flender gear units, T 7300, Table E-am, Flender Code No.     E76        
Mueller Weingarten DT 55 005   CLP 100 CLP 150 CLP 220 CLP 320 CLP 460  

典型性质

Mobilgear 600 XP 68 100 150 220 320 460 680
ISO 粘度等级 68 100 150 220 320 460 680
粘度,ASTM D 445              
mm²/s @ 40 ºC 68 100 150 220 320 460 680
mm²/s @ 100 ºC 8.8 11.2 14.7 19.0 24.1 30.6 39.2
粘度指数, ASTM D2270 101 97 97 97 97 96 90
倾点, °C, ASTM D97 -27 -24 -24 -24 -24 -15 -9
闪点, °C, ASTM D92 230 230 230 240 240 240 285
密度,@15.6 ºC, ASTM D4052, kg/l 0.88 0.88 0.89 0.89 0.90 0.90 0.91
FZG微点蚀,FVA 54,失效阶段/额定   10 / 高 10 / 高 10 / 高 10 / 高 10 / 高 10 / 高
FE 8 磨损试验, DIN 51819-3, D7,5/80-80. 滚柱磨损, mg 2 2 2 2 2 2 2
铁姆肯OK负荷, ASTM D 2782,磅 65 65 65 65 65 65 65
4 球 EP 试验, ASTM D2783,              
焊接负荷,kg 200 200 250 250 250 250 250
负荷磨损指数,kgf 47 47 47 48 48 48 48
FZG划擦,DIN 51354,失效阶段              
A/8.3/90 12+ 12+ 12+ 12+ 12+ 12+ 12+
A/16.6/90   12+ 12+ 12+ 12+ 12+ 12+
防锈保护, ASTM D665,海水 通过 通过 通过 通过 通过 通过 通过
铜片腐蚀,ASTM D130, 3 小时 @ 100 ºC 1B 1B 1B 1B